DOI10.1109/RSETE.2011.5965800
页码6312-6315
英文摘要The semi-solid slurry of AZ91D alloy, produced by a novel self-inoculation method, is isothermal treated. Microstructure evolution and mechanism of microstructure formation during isothermal holding are investigated. The results show that primary α-Mg grains are in small size and present polygon morphology in the slurry. During isothermal holding, the size of particles increases with increasing holding time, while the roundness turns better. But the excessive long holding time is bad for the size and roundness of particles. Deformation of dendrite arm is the primary cause of microstructure formation during pouring, meanwhile, ripening and coarsening during isothermal holding. The nucleus generated from the procedure of melt treatment by self-inoculation, and competitive nucleation in undercooled melt which is near the liquidus during isothermal holding is the main source of primary α-Mg phase. © 2011 IEEE.
会议录2011 International Conference on Remote Sensing, Environment and Transportation Engineering, RSETE 2011 - Proceedings
会议录出版者IEEE Computer Society
语种中文
内容类型会议论文
源URL[http://ir.lut.edu.cn/handle/2XXMBERH/116307]  
专题材料科学与工程学院
省部共建有色金属先进加工与再利用国家重点实验室
作者单位State Key Laboratory of Gansu Advanced Non-Ferrous Metal Materials, Lanzhou University of Technology, Lanzhou, China
推荐引用方式
GB/T 7714
Li, Yuandong,Qu, Junfeng,Xing, Bo,et al. Study of microstructural formation mechanism of AZ91D magnesium alloy melt during semi-solid isothermal holding[C]. 见:.
个性服务
查看访问统计
相关权益政策
暂无数据
收藏/分享
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。


©版权所有 ©2017 CSpace - Powered by CSpace