Microstructural evolution of SiC coating on C/C composites exposed to 1500?▲C in ambient air | |
Zhou, Wei; Xiao, Peng; Luo, Wei; Li, Yang | |
刊名 | Ceramics International |
2019 | |
卷号 | Vol.45 No.1页码:854-860 |
URL标识 | 查看原文 |
公开日期 | [db:dc_date_available] |
内容类型 | 期刊论文 |
URI标识 | http://www.corc.org.cn/handle/1471x/4614878 |
专题 | 湖南大学 |
作者单位 | 1.College of Metallurgy and Materials Engineering, Hunan University of Technology, Zhuzhou 2.412008, China 3.State Key Laboratory of Powder Metallurgy, Central South University, Changsha 4.410083, China |
推荐引用方式 GB/T 7714 | Zhou, Wei,Xiao, Peng,Luo, Wei,et al. Microstructural evolution of SiC coating on C/C composites exposed to 1500?▲C in ambient air[J]. Ceramics International,2019,Vol.45 No.1:854-860. |
APA | Zhou, Wei,Xiao, Peng,Luo, Wei,&Li, Yang.(2019).Microstructural evolution of SiC coating on C/C composites exposed to 1500?▲C in ambient air.Ceramics International,Vol.45 No.1,854-860. |
MLA | Zhou, Wei,et al."Microstructural evolution of SiC coating on C/C composites exposed to 1500?▲C in ambient air".Ceramics International Vol.45 No.1(2019):854-860. |