Inhibited transesterification of PET/PBT blends filled with silica nanoparticles during melt processing | |
Wang, Feng; Meng, Xiangfu; Xu, Xinfeng; Wen, Bin; Qian, Zhongzhong; Gao, Xiaowei; Ding, Yanfen; Zhang, Shimin; Yang, Mingshu | |
刊名 | POLYMER DEGRADATION AND STABILITY
![]() |
2008-08-01 | |
卷号 | 93期号:8页码:1397-1404 |
关键词 | Nanocomposites Poly(Butylene Terephthalate) Poly(Ethylene Terephthalate) Silicas Transesterification |
ISSN号 | 0141-3910 |
DOI | 10.1016/j.polymdegradstab.2008.05.026 |
英文摘要 | The blends of poly(ethylene terephthalate) (PET) and poly(butylene terephthalate) (PBT) undergo transesterification reactions between PET and PBT during melt processing. In this research, PET/PBT transesterification has been investigated in the presence of nano-fillers, including pure SiO2 and silane-coupling-agent-modified SiO2. The results show that the incorporation Of SiO2 nanoparticles inhibits PET/PBT transesterification, and the influence of pure SiO2 is higher than modified SiO2. The inhibition of SiO2 on transesterification is explained by the fact that the hydroxyl end groups of PET and PBT react with the surface hydroxyl groups of SiO2 before transesterification due to the high activity of surface hydroxyl groups of SiO2, and the reduction of hydroxyl end groups of PET and PBT leads to the inhibition of transesterification between PET and PBT. This has been demonstrated by the experimental data of TGA, FTIR, and XPS. And the reactivity of hydroxyl end groups of PBT is higher than that of PET. (C) 2008 Elsevier Ltd. All rights reserved. |
语种 | 英语 |
出版者 | ELSEVIER SCI LTD |
WOS记录号 | WOS:000259388900001 |
内容类型 | 期刊论文 |
源URL | [http://ir.iccas.ac.cn/handle/121111/65073] ![]() |
专题 | 中国科学院化学研究所 |
通讯作者 | Yang, Mingshu |
作者单位 | Chinese Acad Sci, Inst Chem, Beijing Natl Lab Mol Sci, CAS Key Lab Engn Plast, Beijing 100190, Peoples R China |
推荐引用方式 GB/T 7714 | Wang, Feng,Meng, Xiangfu,Xu, Xinfeng,et al. Inhibited transesterification of PET/PBT blends filled with silica nanoparticles during melt processing[J]. POLYMER DEGRADATION AND STABILITY,2008,93(8):1397-1404. |
APA | Wang, Feng.,Meng, Xiangfu.,Xu, Xinfeng.,Wen, Bin.,Qian, Zhongzhong.,...&Yang, Mingshu.(2008).Inhibited transesterification of PET/PBT blends filled with silica nanoparticles during melt processing.POLYMER DEGRADATION AND STABILITY,93(8),1397-1404. |
MLA | Wang, Feng,et al."Inhibited transesterification of PET/PBT blends filled with silica nanoparticles during melt processing".POLYMER DEGRADATION AND STABILITY 93.8(2008):1397-1404. |
个性服务 |
查看访问统计 |
相关权益政策 |
暂无数据 |
收藏/分享 |
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。
修改评论